Density (23°C) | 1.04 | g/cm³ | ISO 1183 |
Melt Volume-Flow Rate (MVR) (275°C/5.0 kg) | 35 | cm³/10min | ISO 1133 |
Mechanical | Nominal Value | Unit | Test Method |
Tensile Modulus | 2300 | MPa | ISO 527-2/1 |
Tensile Stress (Yield) | 55.0 | MPa | ISO 527-2/50 |
Tensile Strain (Break) | 30 | % | ISO 527-2/50 |
Flexural Modulus 1 | 2100 | MPa | ISO 178 |
Flexural Stress 1 | ISO 178 | ||
-- | 80.0 | MPa | |
-- 2 | 65.0 | MPa | |
Flexural Strain at Break 3 | 7.0 | % | ISO 178 |
Impact | Nominal Value | Unit | Test Method |
Charpy Notched Impact Strength (23°C) | 7.0 | kJ/m² | ISO 179/1eA |
Charpy Unnotched Impact Strength (23°C) | No Break | ISO 179/1eU |
Thermal | Nominal Value | Unit | Test Method |
Heat Deflection Temperature | |||
0.45 MPa, Unannealed | 150 | °C | ISO 75-2/B |
1.8 MPa, Unannealed | 65.0 | °C | ISO 75-2/A |
Melting Temperature 4 | 262 | °C | DIN EN 11357-1 |
Flammability | Nominal Value | Unit | Test Method |
Burning Rate 5 (1.00 mm) | <100 | mm/min | FMVSS 302 |
Flame Rating (0.8 mm) | HB | UL 94 |
PA66半透明或不透明乳白色结晶形聚合物,广泛用于制造机械、汽车、化学与电气装置的零件,如齿轮、滚子、滑轮、辊轴、泵体中叶轮、风扇叶片、高压密封围、阀座、垫片、衬套、各种把手、支撑架、电线包层等。亦可制成薄膜用作包装材料。此外,还可用于制作医疗器械、体育用品、日用品等